{"_buckets": {"deposit": "439cd844-a952-46f3-9106-dbabc413d037"}, "_deposit": {"id": "2000788", "owners": [1], "pid": {"revision_id": 0, "type": "depid", "value": "2000788"}, "status": "published"}, "_oai": {"id": "oai:u-ryukyu.repo.nii.ac.jp:02000788", "sets": ["1642838338003", "1642838406845"]}, "author_link": [], "item_1617186331708": {"attribute_name": "Title", "attribute_value_mlt": [{"subitem_1551255647225": "ひずみ情報による非貫通穴材の疲労き裂進展挙動の検知", "subitem_1551255648112": "ja"}, {"subitem_1551255647225": "An Inspection of Fatigue Crack Extension of a Blind-Holed Specimen Based on Strain Information", "subitem_1551255648112": "en"}]}, "item_1617186419668": {"attribute_name": "Creator", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "真壁, 朝敏", "creatorNameLang": "ja"}]}, {"creatorNames": [{"creatorName": "糸数, 真哉", "creatorNameLang": "ja"}]}, {"creatorNames": [{"creatorName": "大場, 克巳", "creatorNameLang": "ja"}]}, {"creatorNames": [{"creatorName": "兼城, 英夫", "creatorNameLang": "ja"}]}, {"creatorNames": [{"creatorName": "Makabe, Chobin", "creatorNameLang": "en"}]}, {"creatorNames": [{"creatorName": "Itokazu, Masaya", "creatorNameLang": "en"}]}, {"creatorNames": [{"creatorName": "Ohba, Katumi", "creatorNameLang": "en"}]}, {"creatorNames": [{"creatorName": "Kaneshiro, Hideo", "creatorNameLang": "en"}]}]}, "item_1617186476635": {"attribute_name": "Access Rights", "attribute_value_mlt": [{"subitem_1522299639480": "open access", "subitem_1600958577026": "http://purl.org/coar/access_right/c_abf2"}]}, "item_1617186499011": {"attribute_name": "Rights", "attribute_value_mlt": [{"subitem_1522650717957": "ja", "subitem_1522651041219": "Copyright (c) 1992 日本機械学会"}]}, "item_1617186609386": {"attribute_name": "Subject", "attribute_value_mlt": [{"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Fatigue"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Blind-Holed Specimen"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Crack Initiation"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Crack Growth"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Crack Opening"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Crack Closing"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Strain Gauge"}, {"subitem_1522299896455": "en", "subitem_1522300014469": "Other", "subitem_1523261968819": "Measurement Method"}]}, "item_1617186626617": {"attribute_name": "Description", "attribute_value_mlt": [{"subitem_description": "A detection of fatigue crack initiation and growth behavior of a blind-holed specimen was carried out by means of the strain interference method. The strains on the center axis of the hole are used for the determination of the strain function \u0027h\u0027. The crack initiation can be detected using the waveform of the strain function \u0027h\u0027. The waveform of \u0027h\u0027 of the precracking can be distinguished from that of the postcracking. The penetration of crack depth into the specimen thickness can also be inspected using the waveform of the strain function \u0027h\u0027. Such variations of the waveform are based on the crack tip opening and closing behavior. Furthermore, the approximate estimation of crack length was carried out using the value of the strain function \u0027hh\u0027 measured at the maximum stress point.", "subitem_description_type": "Other"}, {"subitem_description": "論文", "subitem_description_type": "Other"}]}, "item_1617186643794": {"attribute_name": "Publisher", "attribute_value_mlt": [{"subitem_1522300295150": "ja", "subitem_1522300316516": "日本機械学会"}]}, "item_1617186702042": {"attribute_name": "Language", "attribute_value_mlt": [{"subitem_1551255818386": "jpn"}]}, "item_1617186783814": {"attribute_name": "Identifier", "attribute_value_mlt": [{"subitem_identifier_type": "HDL", "subitem_identifier_uri": "http://hdl.handle.net/20.500.12000/226"}]}, "item_1617186920753": {"attribute_name": "Source Identifier", "attribute_value_mlt": [{"subitem_1522646500366": "ISSN", "subitem_1522646572813": "03875008"}, {"subitem_1522646500366": "NCID", "subitem_1522646572813": "AN0018742X"}]}, "item_1617186941041": {"attribute_name": "Source Title", "attribute_value_mlt": [{"subitem_1522650068558": "ja", "subitem_1522650091861": "日本機械学会論文集. A編"}, {"subitem_1522650068558": "en", "subitem_1522650091861": "Transactions of the Japan Society of Mechanical Engineers. A"}]}, "item_1617187056579": {"attribute_name": "Bibliographic Information", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1992-02-25", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "546", "bibliographicPageEnd": "39", "bibliographicPageStart": "34", "bibliographicVolumeNumber": "58"}]}, "item_1617258105262": {"attribute_name": "Resource Type", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_1617265215918": {"attribute_name": "Version Type", "attribute_value_mlt": [{"subitem_1522305645492": "VoR", "subitem_1600292170262": "http://purl.org/coar/version/c_970fb48d4fbd8a85"}]}, "item_1617605131499": {"attribute_name": "File", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_access", "download_preview_message": "", "file_order": 0, "filename": "kaneshiro_h12.pdf", "future_date_message": "", "is_thumbnail": false, "mimetype": "", "size": 0, "url": {"objectType": "fulltext", "url": "https://u-ryukyu.repo.nii.ac.jp/record/2000788/files/kaneshiro_h12.pdf"}, "version_id": "45aed3e4-8fef-4a16-9c6e-9da4deb9acd5"}]}, "item_title": "ひずみ情報による非貫通穴材の疲労き裂進展挙動の検知", "item_type_id": "15", "owner": "1", "path": ["1642838338003", "1642838406845"], "permalink_uri": "http://hdl.handle.net/20.500.12000/226", "pubdate": {"attribute_name": "PubDate", "attribute_value": "2007-03-04"}, "publish_date": "2007-03-04", "publish_status": "0", "recid": "2000788", "relation": {}, "relation_version_is_last": true, "title": ["ひずみ情報による非貫通穴材の疲労き裂進展挙動の検知"], "weko_shared_id": -1}
  1. 学術雑誌論文
  2. その他
  1. 部局別インデックス
  2. 工学部

ひずみ情報による非貫通穴材の疲労き裂進展挙動の検知

http://hdl.handle.net/20.500.12000/226
http://hdl.handle.net/20.500.12000/226
15acb1a2-3a8e-42bb-b421-f4edb27c8743
名前 / ファイル ライセンス アクション
kaneshiro_h12.pdf kaneshiro_h12.pdf
Item type デフォルトアイテムタイプ(フル)(1)
公開日 2007-03-04
タイトル
タイトル ひずみ情報による非貫通穴材の疲労き裂進展挙動の検知
言語 ja
タイトル
タイトル An Inspection of Fatigue Crack Extension of a Blind-Holed Specimen Based on Strain Information
言語 en
作成者 真壁, 朝敏

× 真壁, 朝敏

ja 真壁, 朝敏

Search repository
糸数, 真哉

× 糸数, 真哉

ja 糸数, 真哉

Search repository
大場, 克巳

× 大場, 克巳

ja 大場, 克巳

Search repository
兼城, 英夫

× 兼城, 英夫

ja 兼城, 英夫

Search repository
Makabe, Chobin

× Makabe, Chobin

en Makabe, Chobin

Search repository
Itokazu, Masaya

× Itokazu, Masaya

en Itokazu, Masaya

Search repository
Ohba, Katumi

× Ohba, Katumi

en Ohba, Katumi

Search repository
Kaneshiro, Hideo

× Kaneshiro, Hideo

en Kaneshiro, Hideo

Search repository
アクセス権
アクセス権 open access
アクセス権URI http://purl.org/coar/access_right/c_abf2
権利情報
言語 ja
権利情報 Copyright (c) 1992 日本機械学会
主題
言語 en
主題Scheme Other
主題 Fatigue
主題
言語 en
主題Scheme Other
主題 Blind-Holed Specimen
主題
言語 en
主題Scheme Other
主題 Crack Initiation
主題
言語 en
主題Scheme Other
主題 Crack Growth
主題
言語 en
主題Scheme Other
主題 Crack Opening
主題
言語 en
主題Scheme Other
主題 Crack Closing
主題
言語 en
主題Scheme Other
主題 Strain Gauge
主題
言語 en
主題Scheme Other
主題 Measurement Method
内容記述
内容記述タイプ Other
内容記述 A detection of fatigue crack initiation and growth behavior of a blind-holed specimen was carried out by means of the strain interference method. The strains on the center axis of the hole are used for the determination of the strain function 'h'. The crack initiation can be detected using the waveform of the strain function 'h'. The waveform of 'h' of the precracking can be distinguished from that of the postcracking. The penetration of crack depth into the specimen thickness can also be inspected using the waveform of the strain function 'h'. Such variations of the waveform are based on the crack tip opening and closing behavior. Furthermore, the approximate estimation of crack length was carried out using the value of the strain function 'hh' measured at the maximum stress point.
内容記述
内容記述タイプ Other
内容記述 論文
出版者
言語 ja
出版者 日本機械学会
言語
言語 jpn
資源タイプ
資源タイプ journal article
資源タイプ識別子 http://purl.org/coar/resource_type/c_6501
出版タイプ
出版タイプ VoR
出版タイプResource http://purl.org/coar/version/c_970fb48d4fbd8a85
識別子
識別子 http://hdl.handle.net/20.500.12000/226
識別子タイプ HDL
収録物識別子
収録物識別子タイプ ISSN
収録物識別子 03875008
収録物識別子
収録物識別子タイプ NCID
収録物識別子 AN0018742X
収録物名
言語 ja
収録物名 日本機械学会論文集. A編
収録物名
言語 en
収録物名 Transactions of the Japan Society of Mechanical Engineers. A
書誌情報
巻 58, 号 546, p. 34-39, 発行日 1992-02-25
戻る
0
views
See details
Views

Versions

Ver.1 2022-01-24 07:44:22.508954
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3